[How is the webbing dyed?]
Release date:[2019/11/18] Read a total of [394] time

The ribbons are bright and colorful, and the quality of the webbing products will be given to the customers through multiple screenings. The colored webbing will undergo a rigorous dyeing process. In order to weave such a gorgeous ribbon, dyeing requires a high level of technology. There are two main methods for dyeing webbing:


One is the application of a wide range of dyeing (conventional dyeing), mainly by placing the webbing in a chemical dye solution. Another method is to use a coating to make the coating into tiny insoluble colored particles to adhere to the fabric (the fiber stock solution is not listed here).


The ribbon dyeing process needs to go through the following points (mainly three points):


The first point: pre-treatment of the webbing; the second point: dyeing of the webbing; the third point: the post-processing of the webbing.


First, the ribbon pre-treatment


1. Pure cotton webbing must be "cooked" before dyeing;


2. The cotton belt will be thoroughly cooked by using chemical materials such as eucalyptus oil and hydrogen peroxide, so that the dye can be evenly distributed on the material during dyeing, for example: dark cotton belt and sensitive color, especially dyed. This is especially true when using a series of cotton webbings such as black, dark blue and cold grey;


3. This process takes about 4-5 hours.


Second, the ribbon dyeing process


1. According to different materials (cotton belt, hemp cotton ribbon, nylon webbing, polyester webbing...), select the corresponding dye (such as reactive dye for cotton belt), and then use computer data to make an appropriate dye formula;


2. According to different materials, choose the appropriate dyeing tank (high-temperature ribbon weaving machine for dyeing polyester ribbon, and ordinary temperature webbing machine for dyeing nylon webbing);


3. Select different dyeing temperatures according to different dyes (such as 20-80 degrees of reactive dyes and 130 degrees of diffusing dyes);


4. Sprinkling time is usually 5-6 hours.


Third, the processing of the ribbon


1. This procedure is very important and will affect the color fastness of many dyes (such as color fastness to washing, wet fastness, etc.). A good fixing procedure will make the color fastness of the webbing reach 4-5;


2. Repeat the cooking of the dyed webbing, boil hot water, wash cold water, etc., and repeat it several times;


3. Then you need to add a fixing oil (such as a dark active dyed webbing);


4. The post-treatment time takes about 4-5 hours.


After understanding the dyeing process of the webbing, I will introduce you to the professional webbing manufacturer, Taixing Hongyang New Material Technology Co., Ltd.


Hongyang now has 6 drawing machines, 10 webbing machines and nearly 100 air-changing machines. The polyester yarns produced by the company have stable quality and fast delivery, and are exported to South Korea, South Africa and other countries. Taixing Hongyang mainly develops, produces and sells: polypropylene high-strength yarn, polypropylene air-changing yarn, polyester air-changing silk, ribbon, etc. With its superior quality and good reputation, it has won unanimous praise from customers!


For more product information, please contact: Liu Xuelian 18914408040 Website: http://lnxnc.cn/


Relevant keywords:
About Hongyuan
Team Style
Enterprise Honor
Recruitment
Product Center
Polypropylene high strength wire
Ribbon
Air Change Wire
News Center
Industry information
Company News
Contact Us
Unified Service Hotline: 0086-0523-87367699
All rights reserved Taixing Hongyang New Material Technology Co., Ltd.
Technical Support::China polypropylene network